Will galvanic corrosion happen between aluminum and steel?

It's likely, but it depends on many different factors liks: 1) area ratio of the metals (big aluminum are vs small steel is better) 2) type of exposure (atmospheric, immersed in water..) 3) type of contact (weld, bolts,...).

I cant really gove you an answer,but what I can give you is a way to a solution, that is you have to find the anglde that you relate to or peaks your interest. A good paper is one that people get drawn into because it reaches them ln some way.As for me WW11 to me, I think of the holocaust and the effect it had on the survivors, their families and those who stood by and did nothing until it was too late.